Ademix 565

Construction Chemicals​

Thermal Insulation

Ademix 565

Thermal Insulation Board Plaster

Thermal Insulation Board Plaster

Cement-Based Polymer and Fiber Reinforced Thermal Insulation Board Plaster

Used as plaster on indoor and outdoor surfaces on top of XPS, EPS, rock wool in jacketing systems.

Provides smooth surfaces for interior and exterior spaces.

Adapts easily to the applied surface.

Can be processed easily and for a long time. 

Has high flexibility due to polymer additives.

Thanks to the fiber reinforcement, it absorbs minor stresses originated by insulation materials. Does not crack.

Bending Strength: ≥ 2 N/mm²
Compressive Strength: ≥ 6 N/mm²
Adhesion Strength (on EPS): ≥ 0.08 N/mm²
Water Absorption: ≥ 0.5 N/mm².minute

Water Vapor Permeability Coefficient: µ ≤ 15

Porous Unit Volume Mass of Hardened Mortar: 1400 ± 200 kg/m³

*The above values are valid for 28 days of performance that was obtained as a result of laboratory experiments.

:

Application Temperature: (+5°C) – (+35°C)
Mixing Ratio: 6-7 lt water / 25 kg powder
Usable period: 2 hours

Readjusting period: 20 minutes

Application Thickness: 1-5 mm

Average Consumption: 4–4.5 kg/m² 

*These values are valid for 23°C and 50% relative humidity. Times may vary depending on ambient conditions.

­ -The application surface should be made clean from dust, dirt, oil, paint residue, and similar foreign matters reducing adherence.

­The thermal insulation board on which the application will be made should be solid, well adhered to the surface, clean, and dry.

­ Gaps between the boards should be filled with insulation material or foam.

25 kg  Thermal Insulation Board Plaster is slowly added to 6-7 lt water. Stirred until a homogeneous mixture is obtained with a trowel or a low-speed mixer, leaving no lumps.The mortar which is rested for 5 minutes is then stirred again and made ready for use.

Prepared plaster is applied to the surface with a steel trowel in 2-3 mm thickness. Plaster mesh is placed on top of applied material by stretching from up to down. The second coat application is done approximately 2-3 hours after this process.

­For eliminating cracking risk, glass-fiber mesh should be applied by overlapping 10 cm on joints.

­Beams, corners, windows, and door frames should be reinforced with additional glass-fiber. 

­Corner profiles should be placed on beam, corner, window, and door frames.

­At least 7 days should pass after the plaster application before applying the coating, painting, etc. on plastered surfaces.

­The surface should be moistened at certain periods within 7 days to increase the performance of the plaster.

­Should not be applied in temperatures below 5°C.

­Should not be applied to surfaces that are directly exposed to sun and wind without protective measures.

­Foreign materials should never be mixed into the mortar.

­-After application, all used tools should be washed with plenty of water before drying.

: 

Do not breathe the product directly, as it is cement-based. Avoid contact with skin and eyes.

TS 13687

Grey
25 kg kraft bag 

: 12 months in dry environment and in original package